Loading data. Please wait
Standard Welding Procedure Specification (SWPS) for 75% Ar/25% CO2 Shielded Flux Cored Arc Welding of Carbon Steel (M-1/P-1, Group 1 or 2), 1/8 inch [3 mm] through 1-1/2 inch [38 mm] Thick, E70T-1M and E71T-1M, in the As-Welded of PWHT Condition, Primarily Plate and Structural Applications
Pages: 33
Publication date: 2018-04-10
Price: 272 vnd
| Standard Welding Procedure Specification (SWPS) for 75% Ar/25% CO2 Shielded Flux Cored Arc Welding of Carbon Steel (M-1/P-1, Group 1 or 2), 1/8 inch [3 mm] through 1-1/2 inch [38 mm] Thick, E70T-1M and E71T-1M, in the As-Welded of PWHT Condition, Primarily Plate and Structural Applications | |
| Document identifier | AWS B2.1-1-020:2018 |
| Publication date | 2018-04-10 |
| Classification | |
| Status | Effective |