This practice is used for the preparation of test specimens for the internal tearing resistance of paper, board and related materials when a force is applied perpendicular to the machine direction. Materials whose structures are highly directional cannot be properly tested in their cross direction according to TAPPI T 414 "Internal Testing Resistance of Paper," because, as a rule, the tear turns toward the machine direction as it proceeds. Consequently, it is usually impossible to make a test tear of such a material truly in the cross direction.
Document identifier
TAPPI T 496 sp-19
Title
Specimen Preparation for Cross Directional Internal Tearing Resistance for Paper, Paperboard and Related Materials
TAPPI Category
Process and Product Quality
Publication date
0000-00-00
International Relationship
History of version
TAPPI T 496 sp-19 * TAPPI T496 sp-13 * TAPPI T496 sp-08 * TAPPI T496