ISO 204:2009 specifies the method for the uninterrupted and interrupted creep tests and defines the properties of metallic materials which can be determined from these tests, in particular the creep elongation and the time of creep rupture, at a specified temperature.The stress rupture test is also covered, as is the testing of notched test pieces.
Document identifier
ISO 204:2009 [ Withdrawn ]
Title
Metallic materials - Uniaxial creep testing in tension - Method of test
ISO Category
TC 164/SC 1: Uniaxial testing
Publication date
2009-06-15
International Relationship
BS EN ISO 204:2009 * DIN EN ISO 204
Latest version
ISO 204:2018
History of version
ISO 204:2018*ISO 204:2009 [ Withdrawn ] * ISO 204:2018 * ISO 204:2009 * ISO 204:1997
Price |
185 vnd |