The data to support AWS B2.1-8-322:2018 for Naval Applications (SWPS-N) have been
derived from the above listed Procedure Qualification Records (PQRs), which were reviewed and validated under the
auspices of the Welding Research Council. This SWPS-N is not valid using conditions and variables outside the ranges
listed. The American Welding Society and Naval Sea Systems Command (NAVSEA) consider that this SWPS-N presents
information for producing an acceptable weld using the conditions and variables listed. This procedure is intended to be
used for full penetration groove welds with consumable inserts. The user needs a significant knowledge of welding and
accepts full responsibility for the performance of the weld and for providing the engineering capability, qualified personnel,
and proper equipment to implement this SWPS-N.
Document identifier
AWS B2.1-8-322:2018
Title
Standard Welding Procedure Specification for Naval Applications (SWPS-N) for Gas Tungsten Arc Welding with Consumable Insert Root of Austenitic Stainless Steel (S-8), 1/8 inch [3 mm] through 1-1/2 inch [38 mm] Thick, MIL-3XX, in the As-Welded Condition, Primarily Pipe for Naval Applications
AWS Category
Standard Welding Procedure Specifications
Publication date
2018-12-01
International Relationship
| Price |