View Sample Alloy Digest Data Sheet (PDF) Since 1952, Alloy Digest has been the leading reference for materials property data on metals and alloys used throughout the world. Featuring graphs, charts and tables, these sheets give facts and figures on composition or characterization, physical and mechanical properties, heat treatment, and machinability.Nicrofer 5219 Nb is a precipitation-hardenable Ni-Cr-Fe alloy containing niobium and molybdenum. The alloy possesses excellent strength to 700 (1300 F), good corrosion resistance, and good weldability. A growing application is bolting and quick closure devices for the chemical process industry.
Document identifier
ASM Ni-531
Title
NICROFER 5219 Nb - Nickel-Base Superalloy
ASM Category
Nickel, Miscellaneous nickel alloy
Publication date
1998-01-01