Covers procedures for designing, preparing, stressing, exposing and inspecting C-ring specimens. These versatile, economical specimens may be used to test a variety of product forms including parts joined by welding. C-ring specimens may be stressed to predeterminded levels, using simple equipment for application of either constant load or constant strain.
Document identifier
ISO 7539-5:1989
Title
Corrosion of metals and alloys - Stress corrosion testing - Part 5: Preparation and use of C-ring specimens
ISO Category
TC 156/WG 2: Stress corrosion cracking
Publication date
1989-12-01
International Relationship
BS EN ISO 7539-5:1995 * BS EN ISO 7539-5:1995