Covers procedures for designing, preparing and using bent-beam test specimens. These specimens may be used to test a variety of product forms (i. e. sheet, plate, flat extruded material, wire or rod). They are espesially suitable for multiple testing and for atmospheric stress corrosion tests; they are usually tested under nominally constant strain conditions. Bent-beam specimens made from high strength materials may fracture rapidly and can be dangerous.
Document identifier
ISO 7539-2:1989
Title
Corrosion of metals and alloys - Stress corrosion testing - Part 2: Preparation and use of bent-beam specimens
ISO Category
TC 156/WG 2: Stress corrosion cracking
Publication date
1989-12-01
International Relationship
BS EN ISO 7539-2:1995 * BS EN ISO 7539-2:1995